摘    要:1 Introduction Ceramicmaterialsareincreasinglyutilizedinstruc turalapplicationswhereharshenvironmentisencoun tered .Theirlowdensity ,highhardness,thermalsta bility,andcorrosionresistancemakethemtoplayanimportantroleinengineeringapplications.However ,cerami…


Study on the Fabrication and Characterization of ZTA-SiCw-TiC Polyphase Ceramics
CHENG Jin-rong,XU Yu-fen,MENG Zhong-Yan.Study on the Fabrication and Characterization of ZTA-SiCw-TiC Polyphase Ceramics[J].Journal of Shanghai University(English Edition),2000,4(2).
Authors:CHENG Jin-rong  XU Yu-fen  MENG Zhong-Yan
Abstract:Novel ZTA/Al2O3-SiCw-TiC polyphase ceramics were fabricated by hot pressing techniques. Phase transformation toughening,particle dispersion and whisker reinforcement have obviously superposed strengthening and toughening effects. It is observed that ZTA20SiCw-20TiC has better comprehensive mechanical properties compared with Al2O3-20SiCw-20TiC. For the optimum processing, the density of ≥99.6 %. The tensile stress in matrix introduced by SiC whisker and TiC could be relaxed by the compress stress produced by tetragonal zirconia(ZrO2 (t)) transformation. TiC formed a continuous skeleton which prevented the grain growth of the matrix. The grain sizes of the matrix became finer with increasing TiC. The major fracture mode of the matrix was transcrystalline cleavage rupture.
Keywords:ZTA  SiC  w  TiC  hot pressing  fracture toughness  flexural strength